BMW SUV X4 (G02, 2019) Front Seatback Frame Weld Defect - Recall 19V-563
What this problem usually means
Recall 19V-563 covers 2019 X4 xDrive30i and M40i models because the front seatback frames may have been improperly welded. A weak weld lets the seatback fold forward or rearward unexpectedly; in a crash, a seatback that gives way cannot restrain the occupant as designed, increasing the risk of injury. The defect is in the frame itself, so there is no adjustment or software fix, and a car can feel completely normal on the road while carrying the defect. Inclusion is by VIN and production records, not by symptoms. The remedy is replacement of the front seats at a dealer, free of charge; the recall began September 27, 2019.
Likely causes
- Front seatback frames improperly welded during production (recall 19V-563)
- A seatback that folds forward or rearward under load instead of restraining the occupant
How to fix it — step by step
- Check your VIN at nhtsa.gov/recalls for recall 19V-563; only listed 2019 X4 models are included
- Do not try to test the weld by forcing the seatback, and do not have trim work done on the seats before the recall is completed
- Book the recall at a BMW dealer, where the front seats are replaced free of charge
- After replacement, confirm recall 19V-563 shows closed for your VIN and keep the paperwork with the car
Did that fix it?
Worked through the steps? Say where you landed - it pinpoints what to do next.
Good - you're done. If it comes back, the causes at the top of this page are where to look first.
This fault usually needs a technician - but this is the part they would test first.
Then the likely broken part is the front seat.
Parts that commonly fix it
- front seatShop at Amazon
What fixed yours?
Fixed this on your machine? Tap what did it - reports from owners set the percentages on this page.
Source: manufacturer / repair documentation. Codes can vary by model — confirm against your manual.
Manual & model number
Working on a specific model? The official BMW manual is on BMW's support site — you'll need your model number.
Find your model number in the owner's manual and on the driver-door jamb label. It's the key to the right manual pages and the right parts.